Resumen
The test can be used to determine whether cold slug or unfused areas are present, to determine the amount of moulded-in stress produced by the moulding process, reveal contamination and to show the quality of the weld. Complete fittings are subjected to a temperature of 150° centigrade in an air-circulating oven for a given time depending on the wall thickness of the fitting. The surfaces of the fitting are examined before and after heating. Cracks, blisters,*delamination or weld opening is measured, expressed as a percentage of the wall thickness.
Informaciones generales
-
Estado: RetiradaFecha de publicación: 1990-11Etapa: Retirada de la Norma Internacional [95.99]
-
Edición: 2Número de páginas: 3
-
Comité Técnico :ISO/TC 138/SC 5ICS :23.040.45
- RSS actualizaciones
Ciclo de vida
-
Anteriormente
RetiradaISO 580:1973
RetiradaISO 2043:1974
-
Ahora
-
Revisada por
PublicadoISO 580:2005