Abstract
The method is based on combustion of the test portion in a refractory crucible in a flow of oxygen in the presence of an accelerator, conversion of the carbon present into carbon dioxide and the sulfur present into sulfur dioxide, and measurement of each gas by infrared absorption. Applies to carbon contents between 0,05 % and 2,5 % and/or sulfur contents between 0,001 % and 0,05 % in direct reduced iron.
-
Status: WithdrawnPublication date: 1992-12
-